1. Normal annealing: 790 - After 810 degrees heat, furnace cooling to 650 degrees, the air cooling - — HB170 - 207 2. Isothermal annealing: 790 810 - degree heat, 710 - 720 degrees, isothermal air cooling - — HB207- 229 3. Is the fire: 900 - 920 - degree heat, air cooling - — HB270 - 390 4. High temperature tempering: 650 700 - degree heat, air cooling - — HB229- 285 5. Quench the fire: the 860 - degree heat, oil quenching - — HRC62- 66 6. Low temperature tempering: 150 - 170 degrees of tempering, air cooling - — HRC61- 66 7. Carbonitriding: 820 830 degrees, a total of 1. 5 - 3 hours, oil quenching, - 60 degrees to - Cryogenic treatment + 70 degrees 150 degrees to + 160 tempering, air cooling - — HRC 67 USES for making all kinds of bearing ring material and rolling body. For example: the production of internal combustion engine, electric locomotives, automobiles, tractors, machine tools, rolling mill, boring machine, mining machinery, general machinery, mechanical transmission and high-speed rotating a high load bearing of steel ball, roller and ring. In addition to do ball bearing, bearing ring thereof, and sometimes also used to make tools, such as punching die, measuring tool.
Custom message
Chat Online 编辑模式下无法使用
Leave Your Message inputting...
Thanks for your message, we will reply you soon in our working time!