Sliding bearing of the main fault knowledge rules - bearing
by:Waxing2020-06-07
1)
Tile surface corrosion: spectrum analysis found that non-ferrous metal element concentration anomaly;
Iron spectrum appeared a lot of non-ferrous metal components in sub-micron wear particles;
Lubricating oil excess moisture, acid value exceeds bid.
2)
Shaft neck surface corrosion: spectrum analysis found that iron concentration is unusual, there are a lot of iron in iron spectrum of submicron particles, water or high acid value oil paint.
3)
Shaft neck surface strain: iron spectrum have iron series cutting grinding grain or black oxide particles, metal surface heat tint.
4)
Tile back micro wear: spectrum analysis found that iron concentration is unusual, there are a lot of iron in iron spectrum wear submicron particles, lubricating oil moisture and acid value anomalies.
5)
Bearing surface strain: iron spectrum found cutting abrasive, abrasive ingredients for non-ferrous metal.